• [口頭報告]Effects of temperature, time, and cooling mode on microstructure and mechanical properties of CCA wire under simulated fire environment
    00
    days
    00
    hours
    00
    minutes
    00
    seconds
    00
    days
    00
    hours
    00
    minutes
    00
    seconds

    [口頭報告]Effects of temperature, time, and cooling mode on microstructure and mechanical properties of CCA wire under simulated fire environment

    Effects of temperature, time, and cooling mode on microstructure and mechanical properties of CCA wire under simulated fire environment
    編號:258 稿件編號:248 訪問權限:僅限參會人 更新:2024-05-15 17:47:14 瀏覽:166次 口頭報告

    報告開始:2024年05月30日 19:30 (Asia/Shanghai)

    報告時間:10min

    所在會議:[S7] Minerals and Advanced Energy Materials ? [S7-2] Evening of May 30th

    暫無文件

    摘要
    The effect of various parameters on the microstructure of CCA wires (Copper-clad aluminum wires) in a fire environment is an important data support for fire investigation and identification work. Due to the complexity of the influencing factors at the fire scene, it is difficult to find the cause of the fire at present. Therefore, this paper simulates the temperature, time, and cooling mode in the fire environment to study its effect on the microstructure and mechanical properties of CCA wires. The results show that the size of the grains on the outer surface of the CCA wires, the morphology and characteristics of the cross-section grains, and the Cu-Al IMCs at the interfaces can be used as a basis for determining the cause of the fire. The composition of the outer surface of CCA wires is CuO from 400°C to 800°C. (1) The effect of temperature on the outer surface of CCA wires is more significant than that of time and cooling method. When the annealing time is 30 min, the maximum diameter of the grains is about 0.15 mm at 400°C, rising to 0.31 mm at 600°C, and reaching 0.58 mm at 800°C. (2) A large number of equiaxed crystals with a diameter of about 10 μm are distributed in the cross-section of the CCA wire at 400°C, and etch pits appear on the surface of the grains at 600°C. Dendritic grains of dendritic crystal morphology are observed in the cross-section at 800°C. (3) IMCs layer (Intermetallic compounds layer) is formed in the Cu-Al interface, and the phase and thickness of the IMCs layer change with increasing temperature.
     
    關鍵字
    Fire, Copper-clad aluminum wire, Grain, Cu-Al interface, Intermetallic compounds
    報告人
    Dandan Zhao
    China University of Mining and Technology

    稿件作者
    Dandan Zhao China University of Mining and Technology
    Xiaohong Wang China University of Mining and Technology
    Peizhong Feng China University of Mining and Technology
    發表評論
    驗證碼 看不清楚,更換一張
    全部評論

    聯系我們

    投稿事宜:張老師
    電話:0516-83995113
    會務事宜:張老師
    電話:0516-83590258
    酒店事宜:張老師
    電話:15852197548
    會展合作:李老師
    電話:0516-83590246
    登錄 注冊繳費 提交摘要 酒店預訂
  • 成人视频